Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® EX39F ABS Highest impact extrusion ABS for sheet and blow molding applications. FDA food contact compliant. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature 23.0 - 60.0 °C |
65.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KFL34XXC Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL34XXC is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature 23.0 - 60.0 °C |
65.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP (Europe-Africa-Middle East) LNP* Lubricomp* MFL36S is a compound based on Polypropylene resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature 23.0 - 60.0 °C |
65.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP PI001 PA 6 (Europe-Africa-Middle East) LNP* LUBRICOMP* PI001 is a compound based on PA 6 resin containing Silicone. Added features include Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature 23.0 - 60.0 °C |
65.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP SFL36 PA12 (Europe-Africa-Middle East) LNP* LUBRICOMP* SFL36 is a compound based on PA 12 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature 25.6 - 93.3 °C |
65.0 µin/in-°F @Temperature 78.0 - 200 °F |
Diameter |
Saint-Gobain Rulon® 1045 Bearing/Seal PTFE Rulon® 1045 is a dull gold material that has an excellent ability to elongate in a flip seal application. Coupled with excellent frictional characteristics, it offers the added benefit of energy .. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -30.0 - 30.0 °C |
65.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -30.0 - 30.0 °C |
65.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -30.0 - 30.0 °C |
65.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -30.0 - 30.0 °C |
65.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature 23.0 - 60.0 °C |
65.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BST42 PA6, Impact Modified, Injection Molded BST42 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® EX39 ABS Highest impact extrusion ABS for sheet and blow molding applications. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 LNP* STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -30.0 - 100 °C |
65.0 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1020 PP SABIC® PPcompound 15T1020. This grade is a general purpose, talc filled, heat stabilized polypropylene resin suitable for injection molded applications. The IMDS ID is 16486973. |
|||
CTE, linear, Transverse to Flow | 117 µm/m-°C @Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 (Asia Pacific) LNP STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |