Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 116 µm/m-°C @Temperature 20.0 °C |
64.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical LI-913 ASA, Injection Molding, High Impact Information Provided by LG Chem |
|||
CTE, linear, Transverse to Flow | 116 µm/m-°C @Temperature 20.0 °C |
64.4 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, Dry as Molded Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
CTE, linear, Transverse to Flow | 116 µm/m-°C @Temperature 23.0 - 60.0 °C |
64.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KA000M POM (Europe-Africa-Middle East) LNP* LUBRICOMP* KA000M is a compound based on Acetal Copolymer resin containg Aramide and Proprietary Lubricant. Added features include Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 116 µm/m-°C @Temperature -30.0 - 100 °C |
64.4 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7727 PP SABIC® PPcompound 7727 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, heat stability, and is used in injection molded applications. The IMDS ID.. |
|||
CTE, linear, Transverse to Flow | 116 µm/m-°C @Temperature 23.0 - 60.0 °C |
64.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp WC003 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABI.. |
|||
CTE, linear, Transverse to Flow | 116 µm/m-°C @Temperature 23.0 - 60.0 °C |
64.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP WC003 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 116 µm/m-°C @Temperature 23.0 - 60.0 °C |
64.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp MFK42AS PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFK42AS is a compound based on PP resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 116 µm/m-°C @Temperature 23.0 - 60.0 °C |
64.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP PB006EQ PA 6 (Europe-Africa-Middle East) LNP *THERMOCOMP* PB006EQ is a compound based on PA 6 containing Glass Bead. Added features include Reduced Moisture. |
|||
CTE, linear, Transverse to Flow | 116 µm/m-°C @Temperature 23.0 - 60.0 °C |
64.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starpylen MFK42AS PP, Glass/Mineral Filled, Injection Molded Starpylen MFK42AS is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding ResinInformation provided by Eurostar. |