Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 105 - 190 µm/m-°C | 58.3 - 106 µin/in-°F | Average value: 139 µm/m-°C Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature 20.0 °C |
58.3 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® KU 2-1446 Polycarbonate + ABS Blend
(discontinued **) Key Features:UnfilledPlatableSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bay.. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C | 58.3 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 1505 Z 000000 PBT PBT, non-reinforced, injection molding, extrusion, impact modified |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C | 58.3 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 2505 000000 PBT PBT, non-reinforced, injection molding, flame retardant |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature 23.0 - 80.0 °C |
58.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® CL402U PBT+PC (Europe-Africa-Middle East) XENOY CL402U has been specially developed for extrusion blowmoulding applications, where higher melt strength is desired. XENOY CL402U is a high impact material combined with good UV resistance perf.. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -30.0 - 30.0 °C |
58.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON WS002I PBT LNP* STAT-KON* WS002I is a compound based on PBT resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, High Impact. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature 20.0 °C |
58.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K224-G4U (Dry) 23% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam BFR460A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East) VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load.. |
|||
CTE, linear, Transverse to Flow | 105 - 125 µm/m-°C @Temperature 55.0 - 160 °C |
58.3 - 69.4 µin/in-°F @Temperature 131 - 320 °F |
Average value: 115 µm/m-°C Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |