Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 9.30 µm/m-°C

@Temperature 23.0 - 1500 °C
5.17 µin/in-°F

@Temperature 73.4 - 2730 °F
Secant Value
Carlisle 201LL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
CTE, linear, Transverse to Flow 9.30 µm/m-°C

@Temperature 23.0 - 1500 °C
5.17 µin/in-°F

@Temperature 73.4 - 2730 °F
Secant Value
Carlisle 201LD Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..