Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific) Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 88.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL REN501 PPE+PS Noryl REN501 resin is an unfilled Post Industrial Recycle (PIR) based injection moldable modified polyphenylene ether blend comprising up to 40% PIR content. Available in black only. |
|||
CTE, linear, Transverse to Flow | 88.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL SE1X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications. |
|||
CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
48.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KFI16 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFI16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Silicone. |
|||
CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
48.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 LNP* LUBRICOMP* RL004 is a copmpound based on Nylon 66 resin containing 20% PTFE. Added feature of this grade includes: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
48.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RX05050 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RX05050 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
48.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
48.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON AX01706 ABS LNP* STAT-KON* AX01706 is a compound based on ABS containing proprietary fillers. Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
48.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON ZEF061XC PPO (Europe-Africa-Middle East) LNP* STATKON* ZEF061XC is a compound based on Polyphenyleneoxide resin containing Glass Fiber, Milled Carbon Fiber and Flame Retardant. Added Features include: Electrically Conductive |
|||
CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
48.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP KB008 Acetal Copolymer LNP THERMOCOMP* KB008 is a compound based on Acetal Copolymer resin containing 40% Glass Bead. |
|||
CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
48.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP WX05505 PBT LNP* Thermocomp* WX05505 is a compound based on Thermoplastic Polyester (PBT) resin containing proprietary fillers. |
|||
CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
48.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP LNP* Thermocomp* MF002S is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
48.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/2 |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
CTE, linear, Transverse to Flow | 88.0 µm/m-°C | 48.9 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
CTE, linear, Transverse to Flow | 88.0 - 88.0 µm/m-°C @Temperature 60.0 - 138 °C |
48.9 - 48.9 µin/in-°F @Temperature 140 - 280 °F |
Average value: 88.0 µm/m-°C Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature 20.0 °C |
48.9 µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
LNP Thermotuf® QF-1006 HI Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
(discontinued **) Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades .. |