Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CY4000 PC+ABS (Europe-Africa-Middle East) Cycoloy* CY4000 resin is an injection moldable, flame retardant PC/ABS blend free of brominated or chlorinated flame resistant additives. Cycoloy CY4000 has excellent flow and balanced impact proper.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Europe-Africa-Middle East) CYCOLOY LG9000 is a low gloss PC+ABS injection moulding grade. LG9000 combines good impact / heat and UV resistance with a low gloss surface appearence. It is suitable for automotive interior applic.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnite® D00 301 PET (European Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East) XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
CTE, linear, Transverse to Flow | 80.0 - 96.0 µm/m-°C | 44.4 - 53.3 µin/in-°F | Average value: 86.1 µm/m-°C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® B 40 FA 000000 Nylon 6, Film Grade PA 6, film grade of high viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide"Appl.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 15 000000 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6, 40% Glass Fiber + Mineral PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 30 HTS 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, very good heat-ageing resistance |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQNH4560 PBT (Asia Pacific) Valox* IQNH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Asia Pacific) |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duranex® 6370B Polybutylene Terephthalate (PBT), Anisotropy improvement, 30% GB filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duranex® 750LD Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® FR 3000 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 97 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3010 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® KU 2-1474 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 64.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® T85 XF Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 130°Cbetter flow than T85PreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® KU 2-7608 Polycarbonate + PBT, Mineral Filled Impact Grade ISO 7792-1-PC/PBT,MHPR,-030,MD10(PC+PBT)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-G4U (Dry) 23% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TV4 230 S PBT-GF15 FR(17) 15% Glass Reinforced, Flame Retardant |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Novamid® 3010SR NAT PA66 Easy Molding Grade |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BS PA6 Product description: Grilon BS is an unreinforced, heat stabilized standard PA6 injection molding grade with normal melt viscosity. Grilon BS has the following important properties: Good flow behavi.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Stanyl® TS250F6D Nylon 46-30% Glass Reinforced (Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Stanyl® TW200F8 (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Stanyl® TW241F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Stanyl® TW275F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, Molydisulfide Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSS/4 PA666 Product description: Grilon TSS/4 is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/4 has the following important properties: Good flow behaviorEas.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBATER BF120 PBT, 20% glass fiber reinforced PBT-GF20Information provided by BARLOG plastics GmbH. |