Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR23 ABS Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
CTE, linear, Transverse to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR23 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
CTE, linear, Transverse to Flow | 79.2 - 110 µm/m-°C | 44.0 - 61.1 µin/in-°F | Average value: 89.6 µm/m-°C Grade Count:9 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
CTE, linear, Transverse to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66 LNP LUBRICOMP* RL004S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 79.2 µm/m-°C @Temperature 25.6 - 93.3 °C |
44.0 µin/in-°F @Temperature 78.0 - 200 °F |
Diameter |
Saint-Gobain Rulon® 123 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
CTE, linear, Transverse to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP RF004H PA 66 LNP* THERMOCOMP* RF004H is a compound based on Nylon 66 containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
CTE, linear, Transverse to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL HIPS3190 HIPS Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only. |