Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CM4219 PC+ABS (Asia Pacific) |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East) Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 910A PC (Europe-Africa-Middle East) LEXAN 910A is a low viscosity flame retardant grade, intended for electrical applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® LI1911R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® OQ1023 PC (Asia Pacific) Lexan OQ1023 resin is an optical high purity PC resin optimized for demanding recordable and rewritable formats (CD-R, DVD-R, DVD-RW). It is also suitable for short cycletime CD and DVD production |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastar DN102 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 925A PC (Europe-Africa-Middle East) Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran.. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 925U PC (Europe-Africa-Middle East) Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXE9925A PC (Asia Pacific) Illuminate / edge glow color effect grade of Lexan 9925A. 9925A is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR .. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® 3200LS Mineral Filled Novolac Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability under very stringent testing. This material is designed to minimize stress on the encapsulated .. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DX09315C PC (Asia Pacific) LNP* Stat-Kon* DX09315C is carbon fiber filled polycarbonate composite with good flow ability, and high level of cleanliness for the most demanding application. A unique feature of this material is .. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Panlite® L-1225Z100 Transparent and Weather Resistant grade Polycarbonate Resin Conforms to SAE regulations. It is an injection molding grade that has slightly high fluidity, weather resistance and mold release property and is bluish-tinted to exhibit clear colorApplications:Co.. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Panlite® LV-2225Y Standard (mold release/ice color grade) Polycarbonate Resin Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required to be slightly high fluidity.Appl.. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1 is a standard 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1 can be used for all applications where a higher modulus is required. NORYL GFN1 is ava.. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
Covestro Apec® 1695 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=158 °CPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
Covestro Apec® 1703 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=171 °CPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
Covestro Apec® 2097 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=202 °CPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Apec® HT KU 1-9354/1 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Lighting, electrical parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially.. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Akulon® K224-G6-FC 99.99.99 PA6-GF30 30% Glass Reinforced, Food Contact Grade |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® KU 2-7609 Polycarbonate + PBT, Mineral Filled Impact Grade ISO 7792-1-PC/PBT,MHPR,-030,MD20(PC+PBT)-blendsimpact modifiedInjection molding grade20% mineral filledPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® AL 2643 Polycarbonate, Injection Grade Easy flowing injection molding grade, UV-stabilized.Applications: Automotive lens applications, fulfills U.S. specification SAE J 576C.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® AL 2647 Polycarbonate, Automotive Lens Injection Grade Easy flowing injection molding grade, UV-stabilized, easy mold release agent.Applications: Automotive lens applications, fulfills U.S. specification SAE J 576C.Information provided by Bayer.As of 1 .. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 7.0 cm3/10 minStructural foam5 % Glass fiber reinforcedNormal fiberChlorine- and bromine-free flame retardantHigh viscosityEasy releaseInjection moldingAvailable in natural (opa.. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat.. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSG-30/4 H black 9839 PA666-GF30 Information provided by EMS Grivory |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30 Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® 1143 Polycarbonate Pseudoplastic behavior and high viscosity extrusion grade with UV stabilizer and easy mold release, special grade for twin-wall sheet.Information provided by Bayer.As of 1 September 2015, Bayer Mate.. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50 Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® RS 6015 BV Nylon 6 Alloy, Glass Fiber + Bead Filled (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |