Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 67.4 µm/m-°C @Temperature -30.0 - 30.0 °C |
37.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp DFZ42P PC LNP* Thermocomp* DFZ42P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the.. |
|||
CTE, linear, Transverse to Flow | 67.3 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON RV00AE PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AE is a compound based on PA 66 rsin containing Long Glass Fiber. Added features include; Easy Molding. |
|||
CTE, linear, Transverse to Flow | 67.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON RX07013 PA 66 (Europe-Africa-Middle East) LNP VERTON * RX07013 is a compound based on Nylon 66 resin containig Long Glass. Added features of this material include: Easy Molding and UV Resistant. |