Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL8483 PC COPOLYMER (Asia Pacific) Lexan* EXL8483 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 80% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)
(Unverified Data**) Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXR123R PC (Europe-Africa-Middle East) Lexan FXR123R Resin |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C | 33.3 - 38.9 µin/in-°F | Average value: 67.9 µm/m-°C Grade Count:11 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® T 3150 XF 000000 PBT + PET, 55% Glass Fiber PBT+PET, 55% glass fibers, injection molding, improved flowability, low tendency to warp, increased temperature peak load, increased strength and increased modulus |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 23.0 - 150 °C |
33.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2310 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP EC004XXC PEI LNP* THERMOCOMP* EC004XXC is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Panlite® BS-8120R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP MF742XXH PP LNP* THERMOCOMP* MF742XXH is a compound based on Polypropylene resin containing Glass Fiber and proprietary antimicrobial additives. This product is best suited for touch surfaces in healthcare app.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Panlite® GV-3430R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin GF 30% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® 3158 Polycarbonate Key Features:Release agentUnfilledSuitable processing methods:Injection moldingExtrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TV4 461 (PBT+PET)-GF30 30% Glass Reinforced |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Novamid® 1015G33-8 NAT PA6-GF33 33% Glass Reinforced, Injection Molding |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Novamid® 3010GN30 NAT PA66-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® G4V-5H nat PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45 Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSGL-40/4 black 9833 PA666-GF40 Product description: Grilon TSGL-40/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 black is characterized by the following key-p.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass/Mineral Reinforced PPA High Performance Polyamide Zytel HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is.. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AK8ST41 PA66, Mineral Reinforced, Impact Modified, Injection Molding Staramide AK8ST41 is an Impact Modified, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® DP 2-7655 Polycarbonate + PET, Mineral Filled Impact Grade Developmental productISO 7792-1-PC/PET,MHPR,-030,MD10(PC+PET)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-HG7 Nylon 66-35% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TR XE 4139 black 9231 PA* Product description: Grilamid XE 4139 black 9231 is an amorphous thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic monomers. Grilamid XE 4139 black 9231 contains a processing a.. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359 |
BASF Ultramid® B3M6 30% Mineral Filled PA6 (Dry) Ultramid B3M6 is a 30% mineral reinforced injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent laser markability. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3WG7 BK 00564 30% Glass Filled PA6 (Dry) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |