Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 150 °C |
28.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 150 °C |
28.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Asia Pacific) Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 150 °C |
28.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 150 °C |
28.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics EXTEM XH1005F TPI Resin (Europe-Africa-Middle East) High Heat Amorphous TPI Blend, Tg 267C, High Continuous Use Temperature (CUT). EFSA Food Contact Approved. Material is UL listed. This material is RoHS compliant and also halogen free according VDE/.. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 150 °C |
28.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 150 °C |
28.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Asia Pacific) Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 150 °C |
28.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 150 °C |
28.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics EXTEM XH1015F TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1015 Resin. EFSA food Contact approved. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 40.0 - 120 °C |
28.3 µin/in-°F @Temperature 104 - 248 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFP36 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFP36 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 20.0 °C |
28.3 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastalloy DA111 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Transverse to Flow | 51.0 - 140 µm/m-°C | 28.3 - 77.8 µin/in-°F | Average value: 87.9 µm/m-°C Grade Count:63 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP JFL24 PES (Europe-Africa-Middle East) LNP* Lubricomp* JFL24 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP JX00061 PES (Europe-Africa-Middle East) LNP* Lubricomp* JX00061 is a compound based on Polyethersulfone resin containing Carbon Fiber, Proprietary Lubricant. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL ZWM2411 PPE+PS (Asia Pacific) Modified PPO*, 30% mineral filled product, V-1@1.5mm, HDT 125degC, low warpage product, BK color only |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp UCL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UCL36AS is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.This data .. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36ASP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UCL36ASP is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
28.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRILOY DF206XXH PC LNP* LUBRILOY* DF206XXH is a compound based on Polycarbonate containing 30% Glass Fiber, Proprietary Lubricant. Added features of this grade include: Wear Resistant, Healthcare. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
28.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp ZWM2411 PPE+PS (Asia Pacific) Modified PPO*, 30% mineral filled product, V-1@1.5mm, HDT 125degC, low warpage product, BK color onlyThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
28.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP EP003 PEI LNP* Lubricomp EP003 is a Polyetherimide containing 15% PTFE/Silicone. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL ZM3242 PPE+PS (Asia Pacific) Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degC |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
28.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RX99732C PA 66 LNP* Thermocomp* PDX-R-99732 is a Nylon 6/6 with proprietary fillers. |
|||
CTE, linear, Transverse to Flow | 51.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp ZM3242 PPE+PS (Asia Pacific) Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degCThis data was supplied by SABIC-IP for the Asia Pacific region. |