Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha.. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend High heat amorphous TPI Blend, Chemical Resistant |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Extem UH1016M TPI Blend High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Extem UH1016M TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 150 °C |
26.1 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1026 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 20.0 °C |
26.1 µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
LNP Lubricomp® EL-4030 Polyetherimide, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 °C |
26.1 µin/in-°F @Temperature 73.4 °F |
ASTM D696 |
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Crystalline
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 °C |
26.1 µin/in-°F @Temperature 73.4 °F |
ASTM D696 |
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 °C |
26.1 µin/in-°F @Temperature 73.4 °F |
ASTM D696 |
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Crystalline
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C | 26.1 µin/in-°F | |
Idemitsu Kosan Xarec® EA 513 SPS, 30% Glass Filled |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C | 26.1 µin/in-°F | |
Idemitsu Kosan Xarec® EA 537 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
26.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
26.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DX11411 PC LNP* STAT-KON* DX11411 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
26.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON UEF26AS PPA (Europe-Africa-Middle East) LNP* Stat-kon* UEF26AS is a compound based on Polyphthalamide resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
26.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP JF003E PES LNP* THERMOCOMP* JF003E is a compound based on Polyethersulfone resin containing 15% Glass Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
26.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Europe-Africa-Middle East) LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 20.0 °C |
26.1 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makroblend® UT-620 G Polycarbonate + Polyester Blend Key Features:Contains FillerHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 Septembe.. |
|||
CTE, linear, Transverse to Flow | 47.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
26.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF OF008EI PPS (Europe-Africa-Middle East) LNP* Thermotuf* OF008EI is a compound based on PPS-Linear resin, containing Glass Fiber. Added features include : High Impact and Easy Molding. |