Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 46.0 µm/m-°C | 25.6 µin/in-°F | ASTM D696 |
Kuraray Genestarâ„¢ G1301A-M61 Nylon, 30% Glass Filled 30% Glass reinforced and impact modified injection grade.Main Features:Higher elongation and impact strengthHeat resistanceChemical resistanceExample of applications:Quick connector |
|||
CTE, linear, Transverse to Flow | 46.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK (Europe-Africa-Middle East) LNP*LUBRICOMP* LFL36 is a compound based on Polyetheretherketone resin containing Glass Fiber, PTFE.
Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-A.. |
|||
CTE, linear, Transverse to Flow | 46.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP UCL16AS PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, containing Carbon Fiber and PTFE. Added features include Heat Stabilized |
|||
CTE, linear, Transverse to Flow | 46.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
25.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DC10EPFR PC LNP* STAT-KON* Lexan_DC10EPFR is a compound based on Polycarbonate containing Carbon Fiber. Added features of this grade include: Exceptional Processing, Flame Retardant, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 46.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon OX92182 PPS (Europe-Africa-Middle East) LNP* STAT-KON* OX92182 is a compound based on PPS-Branched resin containing Glass Fiber, Carbon Fiber, Mineral. Added features include : Electrically Conductive.This data was supplied by SABIC-IP fo.. |
|||
CTE, linear, Transverse to Flow | 46.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
25.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp ZF008 PPO LNP* Thermocomp* ZF008 is a compound based on Modified PPO containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 46.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON MV00AS PP (Europe-Africa-Middle East) LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, heat stabilized |
|||
CTE, linear, Transverse to Flow | 46.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp EF006R PEI (Europe-Africa-Middle East) LNP* Thermocomp* EF006R is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Mold Release.This data was supplied by SABIC-IP for the Europe-A.. |
|||
CTE, linear, Transverse to Flow | 46.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 46.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OC006 is a compound based on PPS - Linear resin containing Carbon Fiber. Added features include : Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 46.0 - 97.0 µm/m-°C | 25.6 - 53.9 µin/in-°F | Average value: 75.9 µm/m-°C Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |