Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
LNP Thermocomp® OF-1006 Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | Average below Tg, Result based on 450GL30; ISO 11359 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® S-7LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices. It offers an alpha par.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® S-7P Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically .. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
25.0 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP159 Synthetic Fabric
(discontinued **) Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit.. |
|||
CTE, linear, Transverse to Flow | 45.0 - 68.0 µm/m-°C | 25.0 - 37.8 µin/in-°F | Average value: 54.5 µm/m-°C Grade Count:4 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
25.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem 2410F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). UL94 V0 and 5VA listing. US FDA and European Food contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
25.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON EX11402 PEI LNP* STAT-KON* EX11402 is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
25.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp JF003L PES LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
25.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
25.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear (Europe-Africa-Middle East) LNP* Thermocomp* OF008 is a compound based on PPS - Linear resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV006S PP (Asia Pacific) LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV006S PP (Europe-Africa-Middle East) LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV006SU PP LNP VERTON* MV006SU is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV006SU PP (Europe-Africa-Middle East) LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East) NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X6151 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Highest impact, high strain to failure, glycol resistant.USES: Water pumps and water pump .. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X640 Resole Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® 46SF5030 PA46-GF30 FR(17) 30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30 Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT1V-45 HY black 9205 PA6T/6I-GF45 Product description: Grivory HT1V-45 HY black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-45 HY .. |
|||
CTE, linear, Transverse to Flow | 45.0 - 80.0 µm/m-°C | 25.0 - 44.4 µin/in-°F | Average value: 62.8 µm/m-°C Grade Count:18 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |