Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 41.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC LNP LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 41.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 41.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP SCP36 PA12 LNP* LUBRICOMP* SCP36 is a compound based on Nylon 12 containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 41.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
22.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP LC008EXP PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LC008EXP is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include Electrically Conductive, Easy Molding. |
|||
CTE, linear, Transverse to Flow | 41.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP VERTON EV008 PEI LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
CTE, linear, Transverse to Flow | 41.0 µm/m-°C | 22.8 µin/in-°F | ASTM D696 |
Kuraray Genestar™ G1300A-M41 Nylon, 30% Glass Filled Glass reinforced injection grade. Main Features:Chemical resistanceHeat resistanceExamples of applications:Gears and bearing retainersIntercooler tank and turbo duct pipe |