Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 40.7 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Stat-kon AE004E ABS LNP* Stat-Kon* AE004E is an ABS compound containing Glass Fiber. Characteristics of this grade are Statically Conductive and Easy Molding.This data was supplied by SABIC-IP for the Americas region... |
|||
CTE, linear, Transverse to Flow | 40.6 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU LNP* THERMOCOMP* GX05482 is a compound based on Polysulfone resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |