Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Average below Tg; ISO 11359 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Average below Tg; ISO 11359 |
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
19.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber PA 6, injection molding grade, 30% milled fibers, UL 94V-2 at 0.8 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, "halogen-free", good heat-ageing resistanceApplication Examples: Medic.. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP EFB26ER PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EFB26ER is a compound based on Polyetherimide containing Glass Fiber, Glass Bead. Added features include: Easy Molding, Mold Release. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature 20.0 °C |
19.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Multilon DN-1530B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 30 % filler. Improved stiffness and high fluidity realizes a thin wall.. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP DC0041PQ PC LNP* THERMOCOMP* DC0041PQ is a compound based on Polycarbonate resin containing Carbon Fiber. Added feature of this grade is: Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp XF006S LNP* Thermocomp* XF006S is a compound based on Amorphous Nylon containing Glass Fiber. Characteristics of this grade are: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP XF006S PA LNP* THERMOCOMP* XF006S is a compound based on Amorphous Nylon containing 30% Glass Fiber. Added feature of th is grade is: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature 20.0 °C |
19.4 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X613 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Solenoid covers or automotive under-bonnet applications such as: water pumps, impeller.. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature 20.0 °C |
19.4 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X620/1 Novolac Phenolic Glass fiber and graphite filled phenolic molding compound with excellent friction properties.USES: Low friction bearings, video recorder and compact disc parts. Not suitable for applications requir.. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature 20.0 °C |
19.4 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X7010 Novolac Phenolic Glass fiber reinforced molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® AV2 390 XT PET GF50 50% Glass Reinforced, Applications with extremely narrow tolerances |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TW271B6 (PA46+PTFE)-CF30 30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30 30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® AV2 390 XL PET GF50 50% Glass Reinforced, Low outgassing |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature 0.000 - 100 °C |
19.4 µin/in-°F @Temperature 32.0 - 212 °F |
z direction; IPC TM-650 2.4.24 |
Arlon CLTE-P Pre-Preg Bonding Layer Arlon's CLTE-P Prepreg Bonding Layer is a ceramic filled PTFE coated glass stock that is used as a bonding ply for CLTE, CLTE-X or CLTE-AT laminates. CLTE-P is a pre-preg material that consists of .. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | z direction |
Arlon TC600 Glass, PTFE and Micro-Dispersed Ceramic High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature 0.000 - 100 °C |
19.4 µin/in-°F @Temperature 32.0 - 212 °F |
z direction; IPC TM-650 2.4.24 |
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a.. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C @Temperature 20.0 °C |
19.4 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X611 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Complex precision parts with thin cross section and good mechanical properties e.g. in.. |
|||
CTE, linear, Transverse to Flow | 35.0 - 100 µm/m-°C | 19.4 - 55.6 µin/in-°F | Average value: 68.7 µm/m-°C Grade Count:7 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
CTE, linear, Transverse to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TC502 PA46 Thermal conductive material |
|||
CTE, linear, Transverse to Flow | 35.0 - 116 µm/m-°C | 19.4 - 64.4 µin/in-°F | Average value: 79.2 µm/m-°C Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |