Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 190 µm/m-°C @Temperature 23.0 - 55.0 °C |
106 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 190 µm/m-°C @Temperature 23.0 - 60.0 °C |
106 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP HX00059 PA11 (Europe-Africa-Middle East) LNP * Lubricomp * HX00059 is a compound based on PA 11 resin, containing a Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 190 µm/m-°C | 106 µin/in-°F | ISO 11359-1/-2 |
DSM Arnitel® XG6029 TPC-ET Extrusion Grade |
|||
CTE, linear, Transverse to Flow | 190 µm/m-°C | 106 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 190 µm/m-°C | 106 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I.. |
|||
CTE, linear, Transverse to Flow | 190 µm/m-°C @Temperature 23.0 - 60.0 °C |
106 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam BFR200Y PA6, Flame Retardant, Injection Molded Starflam BFR200Y is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 190 µm/m-°C | 106 µin/in-°F | ISO 11359-1/-2 |
DSM Arnitel® CM551 TPC-ES Heat Resistant Copolyester |