Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 18.0 - 66.0 µm/m-°C | 10.0 - 36.7 µin/in-°F | Average value: 39.7 µm/m-°C Grade Count:5 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Temperature 20.0 °C |
10.0 µin/in-°F @Temperature 68.0 °F |
Crosswise; ASTM D696 |
G-9 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane.. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Temperature 20.0 °C |
10.0 µin/in-°F @Temperature 68.0 °F |
Crosswise; ASTM D696 |
G-3 Fiberglass Phenolic Laminate Sheet This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of .. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
10.0 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis |
Industrial Laminates/Norplex NP841 Glass Fabric
(discontinued **) Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: .. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
10.0 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP504 Glass Fabric Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note.. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
10.0 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP509 Glass Fabric Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc.. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
10.0 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP664 Paper Base Laminate Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062.. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl TN240 PPE+PS PPE+PS blend. Unfilled. Transparent. Good flow. Scratch resistant. Injection molding. Suitable for housewares, personal care and small appliance applications.This data was supplied by SABIC-IP for t.. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl TN240 PPE+PS (Asia Pacific) PPE+PS. Transparent. High flow, scratch resistant. Injection molding. Housewares and small appliances applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Temperature -30.0 - 100 °C |
10.0 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7985 PP SABIC® PPcompound 7985 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with interior automotive UV stability. The IMDS is 2097.. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
10.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon DE008E PC (Europe-Africa-Middle East) LNP* Stat-kon* DE008E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by SA.. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl PKN4766 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High flow. Extrusion. Microwavable. Food packaging uses.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
10.0 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Temperature 20.0 °C |
10.0 µin/in-°F @Temperature 68.0 °F |
Crosswise; ASTM D696 |
G-5 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-5 has high arc and heat resistance. It used for switch board panels, arc barriers, circuit breaker parts, and .. |
|||
CTE, linear, Transverse to Flow | 18.0 - 27.0 µm/m-°C | 10.0 - 15.0 µin/in-°F | Average value: 23.0 µm/m-°C Grade Count:4 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |
|||
CTE, linear, Transverse to Flow | 18.0 µm/m-°C @Temperature 20.0 °C |
10.0 µin/in-°F @Temperature 68.0 °F |
XY-direction; ASTM D696 |
Premix Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC
(discontinued **) Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression mo.. |