Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 43.0 - 67.0 µm/m-°C @Temperature 50.0 - 300 °C |
23.9 - 37.2 µin/in-°F @Temperature 122 - 572 °F |
Average value: 54.5 µm/m-°C Grade Count:2 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |