Polymer Property : CTE, linear, Transverse to Flow = 151 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 129 - 151 µm/m-°C
71.7 - 83.9 µin/in-°F
Average value: 141 µm/m-°C Grade Count:7
Overview of materials for Cellulose Acetate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr..