Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 20.0 - 139 µm/m-°C | 11.1 - 77.2 µin/in-°F | Average value: 59.8 µm/m-°C Grade Count:4 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |