Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 36.0 - 125 µm/m-°C
20.0 - 69.4 µin/in-°F
Average value: 77.1 µm/m-°C Grade Count:18
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
CTE, linear, Transverse to Flow 90.0 - 125 µm/m-°C

@Temperature 100 - 200 °C
50.0 - 69.4 µin/in-°F

@Temperature 212 - 392 °F
Average value: 108 µm/m-°C Grade Count:2
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
CTE, linear, Transverse to Flow 105 - 125 µm/m-°C

@Temperature 55.0 - 160 °C
58.3 - 69.4 µin/in-°F

@Temperature 131 - 320 °F
Average value: 115 µm/m-°C Grade Count:2
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..