Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 99.1 - 99.1 µm/m-°C @Temperature 26.0 - 200 °C |
55.1 - 55.1 µin/in-°F @Temperature 78.8 - 392 °F |
Average value: 99.1 µm/m-°C Grade Count:1 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||