Polymer Property : CTE, linear, Transverse to Flow = 79.2 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 79.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® FR23 ABS
Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated.
CTE, linear, Transverse to Flow 79.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® FR23 ABS (Asia Pacific)
Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated.
CTE, linear, Transverse to Flow 79.2 - 110 µm/m-°C
44.0 - 61.1 µin/in-°F
Average value: 89.6 µm/m-°C Grade Count:9
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
CTE, linear, Transverse to Flow 79.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66
LNP LUBRICOMP* RL004S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant.
CTE, linear, Transverse to Flow 79.2 µm/m-°C

@Temperature 25.6 - 93.3 °C
44.0 µin/in-°F

@Temperature 78.0 - 200 °F
Diameter
Saint-Gobain Rulon® 123 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
CTE, linear, Transverse to Flow 79.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF004H PA 66
LNP* THERMOCOMP* RF004H is a compound based on Nylon 66 containing 20% Glass Fiber. Added feature of this grade is: Healthcare.
CTE, linear, Transverse to Flow 79.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL HIPS3190 HIPS
Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only.