Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® C6850REC PC+ABS (Europe-Africa-Middle East) PC+ABS Industrial quality. Flame retardant. Limited colors only (Black and Grey)This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
38.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp DBL14 PC (Europe-Africa-Middle East) Internally lubricated Polycarbonate compound, comtaining Glass Bead and PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature 20.0 °C |
38.3 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® GR630 30% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron GR630 is a 30% glass fiber reinforced polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This balance of engineering.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Colorcomp DX98735 PC LNP COLORCOMP* DX98735 is a compound based on Polycarbonate resin containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP COLORCOMP DX98735H PC LNP* COLORCOMP* DX98735H is an unfilled Polycarbonate resin. Added feature of this grade is: Healthcare. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 69.0 - 90.0 µm/m-°C | 38.3 - 50.0 µin/in-°F | Average value: 75.1 µm/m-°C Grade Count:7 |
Overview of materials for Epoxy, Molded, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature 20.0 °C |
38.3 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® 3100LS Mineral Filled Conventional Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A semiconductor grade encapsulant suitable for a wide range of applications ranging from small SOICs to moderate lead count DIPs... |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature 20.0 °C |
38.3 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® 3300SH Mineral Filled Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics and low flash. This compound is especially.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66 LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP AX04518 ABS LNP* THERMOCOMP* AX04518 is a compound based on ABS resin containing proprietary filler(s). |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
38.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DX06094 PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DX06094 is a compound based on Polycarbonate resin containing Glass Fiber . Added features include: High Impact, Non- Brominated & Non-Chlorinated Flame Retardant and Mold Release... |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DX11354 PC (Asia Pacific) This is a PC compound with good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature 20.0 °C |
38.3 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Sumitomo Bakelite North America RX® 431 Cellulose Reinforced Phenolic Novolac RX431 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP D7001IXH PC LNP* THERMOCOMP* D7001IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare ap.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP D7002IXH PC LNP* THERMOCOMP* D7002IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces, housings, etc., in healthcare an.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature 20.0 °C |
38.3 µin/in-°F @Temperature 68.0 °F |
|
Toyobo TS301 PPS, 30% Glass Fiber Reinforced Key Feature: Excellent impact resistance, high flowHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
38.3 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature 20.0 °C |
38.3 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® GR630 HS 30% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron GR630 HS is a heat stabilized, 30% glass fiber reinforced polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This ba.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C | 38.3 µin/in-°F | TMA |
Vyncolit Neopreg Kinel® SK60 L8G Glass Fiber Reinforced Molding Compound High flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited fo.. |
|||
CTE, linear, Transverse to Flow | 69.0 µm/m-°C @Temperature 20.0 °C |
38.3 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® 3300S Mineral Filled Novolac Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, flame retardant, novolac hardened epoxy molding compound designed to provide hermeticity protection exceeding that .. |