Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 64.6 µm/m-°C @Temperature 20.0 °C |
35.9 µin/in-°F @Temperature 68.0 °F |
ASTM E228 |
Polystrand ThermoPro™ IE6010 Unitape Unidirectional Polypropylene-Glass Composite Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer .. |
|||
CTE, linear, Transverse to Flow | 64.6 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36P PC LNP* Lubricomp* DFL36P is a compound based on Polycarbonate containing 30% Glass Fiber 15% PTFE. Added features include: Exceptional Processing. Internally Lubricated. |