Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX2289 PC Lexan* LUX2289 resin is an injection molding grade with high light reflectance |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East) Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makroblend® UT-408 Polycarbonate + Polyester Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34EH PC LNP* LUBRICOMP* DFL34EH is a compound based on Polycarbonate containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Easy Molding, Healthcare, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® AMC2 (132.203) Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound specifically formulated for packaging stress-sensitive devices in DIPs, SOICs, PLCCs and small QFPs. F.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RFL449 PA 66 LNP* LUBRICOMP* RFL449 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA12 LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
35.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon DD0009XQ PC (Europe-Africa-Middle East) LNP* Stat-Kon* DD0009XQ is a compound based on Polycarbonate containing Carbon Powder and Flame Retardant. Added features include Electrically Conductive, Flame Retardant and Easy Molding.This data.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DD000CEX PC LNP STAT-KON* DD000CEX is a compound based on Polycarbonate resin containing Carbon. Added features of this material include: Clean Compounding System. Easy Molding, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DD000CEX PC (Asia Pacific) LNP* STAT-KON* DD000CEX is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 25.6 - 93.3 °C |
35.0 µin/in-°F @Temperature 78.0 - 200 °F |
Diameter |
Saint-Gobain Rulon® 957 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RC006XXH PA 66 LNP* THERMOCOMP* RC006XXH is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RX09411H PA 66 LNP* Thermocomp* RX09411H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
35.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UX06003 PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UX06003 is a compound based on Polyphalamide resin containing Carbon Fiber. Added features include Electrically Conductive, Mold Release, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP VERTON MV00ES PP LNP* VERTON* MV00ES is primarily a concentrate used for blending purposes. This is a 70% long glass fiber Polypropylene compound. Added features of this grade are: Heat Stabilized |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP 40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Asia Pacific) 40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP 9X02841 PBT+PC LNP* Thermocmop* 9X02841 is a PBT/Polycarbonate blend containing proprietary fillers. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
35.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RC00A PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC00A is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive |
|||
CTE, linear, Transverse to Flow | 63.0 - 65.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 - 36.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Verton RV008ESV PA 66 40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
|
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
|
Toyobo TS401 PPS, 40% Glass Fiber Reinforced Key Feature: General Purpose Grade - balanced characteristics suitable for a broad range of uses.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a spec.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C | 35.0 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 20.0 - 93.3 °C |
35.0 µin/in-°F @Temperature 68.0 - 200 °F |
Normal to Laminate |
CIP Composites 200 Series Laminated Polymer Bearing Material The 200 series consists of PTFE/polyester combination fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated ma.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 20.0 - 93.3 °C |
35.0 µin/in-°F @Temperature 68.0 - 200 °F |
Normal to Laminate |
CIP Composites 100 Series Laminated Polymer Bearing Material The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
35.0 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXN PA 66 LNP* THERMOCOMP* RF007SXN is a Hydro-Stable, 35% Glass Fiber reinforced compound based on Nylon 66. Added features of this grade include: Heat Stabilized, NSF Listed. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP VERTON RV00CEXS PA 66 LNP* VERTON* RV00CEXS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural. |