Polymer Property : CTE, linear, Transverse to Flow = 56.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CM5820 PC+ABS (Asia Pacific)
Cycoloy CM5820 resin is a Mineral Filled Non-FR PC+ABS blend with high impact, high modulus, good chemical resistance & improved surface aesthetic, designed for hand help device chassis that require..
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP FARADEX DS0036I PC
LNP* FARADEX* DS0036I is a compound based on Polycarbonate resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, No..
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Faradex DS0036IP PC
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Asia Pacific)
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Europe-Africa-Middle East)
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
31.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP 9X06030 PA 46 (Europe-Africa-Middle East)
LNP* LUBRICOMP* 9X06030 is a compound based on PA46 resin containing PTFE and Carbon Fiber. Added features include: Internally Lubricated, Heat Stabilized.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature 20.0 °C
31.1 µin/in-°F

@Temperature 68.0 °F
Cookson Group Plaskon® 1002 Conventional Encapsulant  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low cost, low stress, conventional molding compound recommended for high volume commodity-type packages that house simple linea..
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature 20.0 °C
31.1 µin/in-°F

@Temperature 68.0 °F
Cookson Group Plaskon® SMT-B-1RC (146.403) Epoxy Molding Compound for PBGAs  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi..
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
31.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP ZFL24 PPE+PS
LNP* LUBRICOMP* ZFL24 is a compound based on PPE+PS resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is: Wear Resistant.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
31.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Lubricomp ZFL24 PPO
LNP* Lubricomp* ZFL24 is a compound based on Modified Polyphenylene Oxide (PPO) containing glass fiber and PTFE lubricant. Characteristics of this grade are: Internally Lubricated.This data was su..
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON ZX08301 PPE (Asia Pacific)
Stat-Kon* ZX08301 compound is a high heat compounds with ESD safe and low warpage performance suitable for use in Semiconductor Packaging Applications.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
31.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS
LNP* THERMOCOMP* CX05470 is a compound based on Polystyrene resin containing 20% Glass Fiber.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
31.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RF009S PA 66
LNP* THERMOCOMP* RF009S is a compound based on Nylon 66 resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized.
CTE, linear, Transverse to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ISO 11359-1/-2
Covestro Bayblend® T90 MF-20* Polycarbonate + ABS, Mineral Filled
Developmental productInjection molding grade20 % mineral filledvery good flowreduced coefficient of thermal dilatationtensile modulus = 5200 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content
CTE, linear, Transverse to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® DP T 7140 LDS 000000 PBT + PET, 44% Mineral + L227Glass Fiber  (discontinued **)
PET+PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimension stability
CTE, linear, Transverse to Flow 56.0 - 150 µm/m-°C

@Temperature 50.0 - 250 °C
31.1 - 83.3 µin/in-°F

@Temperature 122 - 482 °F
Average value: 104 µm/m-°C Grade Count:5
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..