Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 49.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C7122 PC+ABS (Asia Pacific) Cycoloy*C7122 is a mineral filled, non-halogenated flame retardant PC/ABS. Good stiffness with balanced flow and impact performance. |
|||
CTE, linear, Transverse to Flow | 49.0 µm/m-°C @Temperature 20.0 °C |
27.2 µin/in-°F @Temperature 68.0 °F |
ASTM E381 |
Solvay Specialty Polymers Veradel® A-100, A-200, A-300 Polyethersulfone
(discontinued **) For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N.. |
|||
CTE, linear, Transverse to Flow | 49.0 - 65.0 µm/m-°C | 27.2 - 36.1 µin/in-°F | Average value: 58.0 µm/m-°C Grade Count:4 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
CTE, linear, Transverse to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | |
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified |
|||
CTE, linear, Transverse to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | |
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993 |
|||
CTE, linear, Transverse to Flow | 49.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Europe-Africa-Middle East) LNP* Lubricomp* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. |
|||
CTE, linear, Transverse to Flow | 49.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP LX82803 PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LX82803 is a compound based on Polyetheretherketone resin containing Proprietary Lubricant. Added features include : Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 49.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36A PPS - Branched (Europe-Africa-Middle East) LNP* Lubricomp* OCL4036 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 49.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY DX08333 PC (Asia Pacific) LNP Lubriloy* DX08333 is an internally lubricated compound based on Lexan* Polycarbonate resin. Added features of this material include: ESD Safe, PTFE-free Wear & Friction solution and balanced mec.. |
|||
CTE, linear, Transverse to Flow | 49.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing Glass Fiber. Added features include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 49.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp LF004 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LF004 Is a compound based on Polyetheretherketone containg Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 49.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.2 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 228 |
DuPont Performance Polymers VESPEL TP-8395 Polyimide DuPont Vespel TP-8395 parts are specified for high-temperature and high-wear applications. TP-8395 parts offer an excellent balance of mechanical and thermal properties for superior performance in a.. |