Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 48.0 µm/m-°C @Temperature 20.0 °C |
26.7 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastapak 7352 PET
(discontinued **) Unreinforced Low IV. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
CTE, linear, Transverse to Flow | 48.0 µm/m-°C @Temperature 20.0 °C |
26.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1, -2 |
LNP Thermocomp® LF-1006 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
CTE, linear, Transverse to Flow | 48.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL ZM3640 PPE+PS (Asia Pacific) |
|||
CTE, linear, Transverse to Flow | 48.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
26.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DE003Z PC LNP STAT-KON* DE003Z is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Extrusion Grade. |
|||
CTE, linear, Transverse to Flow | 48.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
26.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON RE006 PA 66 LNP STAT-KON* RE006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 48.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
26.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp 9X06477 SPS LNP* Thermocomp* 9X06477 is a compound based on Syndiotactic Polystyrene resin containing Glass Fiber. Characteristics of this grade is Heat Stabilized.This data was supplied by SABIC-IP for the Am.. |
|||
CTE, linear, Transverse to Flow | 48.0 µm/m-°C @Temperature 20.0 °C |
26.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Multilon DN-1520B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 20 % filler. Improved stiffness and high fluidity realizes a thin wall.. |
|||
CTE, linear, Transverse to Flow | 48.0 µm/m-°C @Temperature 20.0 °C |
26.7 µin/in-°F @Temperature 68.0 °F |
|
Toyobo TS201 HS PPS, Glass Fiber/Mineral Reinforced Key Feature: High stiffness, high toughnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excel.. |
|||
CTE, linear, Transverse to Flow | 48.0 µm/m-°C @Temperature 20.0 °C |
26.7 µin/in-°F @Temperature 68.0 °F |
|
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel.. |
|||
CTE, linear, Transverse to Flow | 48.0 µm/m-°C | 26.7 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TC154 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
CTE, linear, Transverse to Flow | 48.0 µm/m-°C | 26.7 µin/in-°F | z, below Tg; IPC TM-650 2.4.24 |
Arlon 84N Polyimide Laminate and Prepreg 84N is a high performance ceramic-filled polyimide prepreg based on Arlon's 85N pure polyimide system, designed for use in filling etched areas in polyimide multilayers that contain thick copper lay.. |
|||
CTE, linear, Transverse to Flow | 48.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
26.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP VERTON RV0079 PA 66 LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing 35% Long Glasss Fiber. Added features of this material include: Flame Retardant, Structural. |