Polymer Property : CTE, linear, Transverse to Flow = 46.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 46.0 µm/m-°C
25.6 µin/in-°F
ASTM D696
Kuraray Genestarâ„¢ G1301A-M61 Nylon, 30% Glass Filled
30% Glass reinforced and impact modified injection grade.Main Features:Higher elongation and impact strengthHeat resistanceChemical resistanceExample of applications:Quick connector
CTE, linear, Transverse to Flow 46.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
25.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK (Europe-Africa-Middle East)
LNP*LUBRICOMP* LFL36 is a compound based on Polyetheretherketone resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-A..
CTE, linear, Transverse to Flow 46.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
25.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP UCL16AS PPA (Europe-Africa-Middle East)
Internally lubricated Polyphthalamide compound, containing Carbon Fiber and PTFE. Added features include Heat Stabilized
CTE, linear, Transverse to Flow 46.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
25.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DC10EPFR PC
LNP* STAT-KON* Lexan_DC10EPFR is a compound based on Polycarbonate containing Carbon Fiber. Added features of this grade include: Exceptional Processing, Flame Retardant, Electrically Conductive.
CTE, linear, Transverse to Flow 46.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
25.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon OX92182 PPS (Europe-Africa-Middle East)
LNP* STAT-KON* OX92182 is a compound based on PPS-Branched resin containing Glass Fiber, Carbon Fiber, Mineral. Added features include : Electrically Conductive.This data was supplied by SABIC-IP fo..
CTE, linear, Transverse to Flow 46.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
25.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp ZF008 PPO
LNP* Thermocomp* ZF008 is a compound based on Modified PPO containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 46.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
25.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV00AS PP (Europe-Africa-Middle East)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, heat stabilized
CTE, linear, Transverse to Flow 46.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
25.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp EF006R PEI (Europe-Africa-Middle East)
LNP* Thermocomp* EF006R is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Mold Release.This data was supplied by SABIC-IP for the Europe-A..
CTE, linear, Transverse to Flow 46.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
25.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber.
CTE, linear, Transverse to Flow 46.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
25.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear (Europe-Africa-Middle East)
LNP* THERMOCOMP* OC006 is a compound based on PPS - Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.
CTE, linear, Transverse to Flow 46.0 - 97.0 µm/m-°C
25.6 - 53.9 µin/in-°F
Average value: 75.9 µm/m-°C Grade Count:12
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Copyright © lookpolymers.com All Rights Reserved