Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 40.0 - 80.0 µm/m-°C | 22.2 - 44.4 µin/in-°F | Average value: 58.0 µm/m-°C Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K-FHG12 (Dry) 60% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K223-KM6 Nylon 6-30% Mineral Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 40.0 - 102 µm/m-°C | 22.2 - 56.7 µin/in-°F | Average value: 61.4 µm/m-°C Grade Count:16 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 23.0 - 150 °C |
22.2 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 4001 PEI (Europe-Africa-Middle East) PTFE filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Baygal® 90 IK 51 Polyurethane Uses: Suitable for the solid insulation of measuring transducers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its ne.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-HM8 (Dry) 40% Mineral Reinforced, Heat Stabilized Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GVL-6H nat PA*-GF60 Product description: Grivory GVL-6H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H na.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50 Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HTV-6H1 black 9205 PA6T/6I-GF60 Product description: Grivory HTV-6H1 black 9205 is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60 Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following .. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-HM8 Nylon 66-40% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® AV2 370 XL PET-GF35 35% Glass Reinforced, Low Outgassing |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GVL-6H black 9915 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50 Product description: Grivory HT1V-5 HY black 9205 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-5 HY bl.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT1V-6 FWA black 9225 PA6T/6I-GF60 Product description: Grivory HT1V-6 FWA black 9225 is a 60 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ASTM E 831 |
Arlon Thermabond® 48991A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation IIa Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style .. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | z direction |
Arlon AD430 Glass, PTFE and Micro-Dispersed Ceramic High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear, Transverse to Flow | 40.0 - 90.0 µm/m-°C | 22.2 - 50.0 µin/in-°F | Average value: 73.6 µm/m-°C Grade Count:39 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
CTE, linear, Transverse to Flow | 40.0 - 80.0 µm/m-°C | 22.2 - 44.4 µin/in-°F | Average value: 59.3 µm/m-°C Grade Count:21 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TS200F10 PA46-GF50 50% Glass Reinforced |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |