Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
TMA; ASTM E831
LNP Thermocomp® LF-1006 EM Polyetheretherketone, Glass Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
CTE, linear, Transverse to Flow 36.0 - 125 µm/m-°C
20.0 - 69.4 µin/in-°F
Average value: 77.1 µm/m-°C Grade Count:18
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
CTE, linear, Transverse to Flow 36.0 - 60.0 µm/m-°C
20.0 - 33.3 µin/in-°F
Average value: 50.3 µm/m-°C Grade Count:14
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
CTE, linear, Transverse to Flow 36.0 - 70.0 µm/m-°C

@Temperature 50.0 - 300 °C
20.0 - 38.9 µin/in-°F

@Temperature 122 - 572 °F
Average value: 51.9 µm/m-°C Grade Count:10
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
CTE, linear, Transverse to Flow 36.0 µm/m-°C
20.0 µin/in-°F
ASTM D696
Kuraray Genestarâ„¢ G1500A-M61 Nylon, 50% Glass Filled
50% Glass reinforced injection grade. Main Features:High strengthHeat resistanceExamples of applications:Structural partsSteel alternating parts
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
20.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP JCL36 PES (Europe-Africa-Middle East)
LNP* LUBRICOMP* JCL36 is a compound based on Polyethersulfone resin containing Carbon Fiber, PTFE. Added features include : Internally Lubricated, Electrically Conductive.
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
20.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP LFL36E PEEK
LNP* LUBRICOMP* LFL36E is a compound based on Polyetheretherketone containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Wear Resistant, Easy Molding.
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
20.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 3452 PEI (Europe-Africa-Middle East)
45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. Resin is RoHS compliant. UL94 V0 and 5VA listing in recognized colors.
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature -40.0 - 150 °C
20.0 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP EC008PXQ PEI
LNP* THERMOCOMP* EC008PXQ is a compound based on Polyetherimide containing 40% Carbon FIber. Added features include: Electrically Conductive, Exceptional Processing
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
20.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP UFW49RS PPA (Europe-Africa-Middle East)
LNP* Thermocomp* UFW49RS is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
20.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP UFW49RSC PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UFW49RSC is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features include: Heat Stabilized.
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
20.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP WCL36 PBT
LNP* LUBRICOMP* WCL36 is a compound based on PBT resin containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant.
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
20.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66
LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Proprietary Fillers. Characteristics of this grade are: Healthcare.
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature 150 °C
20.0 µin/in-°F

@Temperature 302 °F
ASTM E 228
DuPont Performance Polymers VESPEL TP-8556 Polyimide
Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Perform..
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
20.0 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN FR55G50NHLW BK046 Polyphthalamide (PPA)  (Unverified Data**)
55% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Low Warpage and High Stiffness Zytel HTNFR55G50NHLW BK046 is a 50% glass reinforced flame retardant high perf..
CTE, linear, Transverse to Flow 36.0 µm/m-°C
20.0 µin/in-°F
ISO 11359
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry)
Ultramid B3WGM24 BK30564 is a 30% glass/mineral filled heat stabilized injection molding PA6 grade for industrial articles having medium to high rigidity and high dimensional stability.
CTE, linear, Transverse to Flow 36.0 - 110 µm/m-°C
20.0 - 61.1 µin/in-°F
Average value: 59.8 µm/m-°C Grade Count:3
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
TMA; ASTM E831
LNP Thermocomp® JF-1006 E LE BK8-055 Polyethersulfone, Glass Fiber Reinforcement  (discontinued **)
Features: High Viscosity, Low ExtractablesForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L..
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Thickness 1.60 mm
20.0 µin/in-°F

@Thickness 0.0630 in
ASTM D696
E-Polymers SEPAZ® C230GI 30% Glass Fiber Reinforced Good Impact LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..