Polymer Property : CTE, linear, Transverse to Flow = 26.8 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 26.8 - 55.0 µm/m-°C
14.9 - 30.6 µin/in-°F
Average value: 39.8 µm/m-°C Grade Count:22
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
CTE, linear, Transverse to Flow 26.8 µm/m-°C

@Temperature 20.0 °C
14.9 µin/in-°F

@Temperature 68.0 °F
TMA
Sumitomo Bakelite North America RX® 660 Fiberglass Reinforced Phenolic Novolac
RXÂ 660 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitom..