Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 17.0 - 80.0 µm/m-°C | 9.44 - 44.4 µin/in-°F | Average value: 55.4 µm/m-°C Grade Count:12 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
CTE, linear, Transverse to Flow | 17.0 - 50.0 µm/m-°C | 9.44 - 27.8 µin/in-°F | Average value: 36.3 µm/m-°C Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
CTE, linear, Transverse to Flow | 17.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
9.44 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP610 Paper Base Laminate Description: Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.Thickne.. |
|||
CTE, linear, Transverse to Flow | 17.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
9.44 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP611 Paper Base Laminate Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a.. |