Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 150 µm/m-°C @Temperature 23.0 - 55.0 °C |
83.3 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6 PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C @Temperature 23.0 - 55.0 °C |
83.3 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 215 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning .. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 215 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning .. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C @Temperature 23.0 - 55.0 °C |
83.3 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EM630 63 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EM630-H Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® PL380 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® PL381 Injection Molding Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® PL381 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
DSM Arnitel® PL381-H TPC-ET Injection Molding |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® PM381 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
DSM Arnitel® VT3104 TPC-ET Extrusion Grade |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 2S 25 W 20 HL X nat PA610 Product Description: Grilamid 2S 25 W 20 HL X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified and plasticized Polyamide 610, espcailly suitable for extrusion applic.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 2S 25 W 20 X black 9992 PA610-I Product Description: GRILAMID 2S 25 W 20 X black 9992 is a semi-flexible high viscosity heat and impact modified polyamide 610, especially suitable for extrusion applications. This PA610 product is .. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® AZ 3/2 PA66 Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BRZ 247 W PA6 Product description: Grilon BRZ 247 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 247 W has the following important properties: High flexibi.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25 NZ ESD PA12 Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of .. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LV-2A NZ PA12-GF20 Product description: Grilamid LV-2A NZ is a high viscosity polyamide 12 with 20% glass fibers and improved hydrolysis resistance compared to standard polyamide 12 materials. Grilamid LV-2A NZ has a .. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LV-2H PA12-GF20 Product description: Grilamid LV-2H is a 20% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LV-30H FWA black 9225 PA12-GF30 Product description: Grilamid LV-30H FWA black 9225 is a 30 % glass fiber reinforced, heat stabilized polyamide12 injection molding grade with the following special features: Stiffness combined with.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSZ 1 PA666 Product description: Grilon TSZ 1 is a heat stabilized, normal viscosity, impact modified PA66 + PA6 injection molding grade. Grilon TSZ 1 has the following important properties: Excellent flow beha.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSZ 3 PA666 Product description: Grilon TSZ 3 is a heat stabilized, normal viscosity, high impact modified PA66 + PA6 injection molding grade. Grilon TSZ 3 has the following important properties: Excellent toug.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4128 black 9221 PA610 Product description: Grilamid XE 4128 black 9221 is a modified high viscosity Polyamide 610 for extrusion as well as injection molding. A characteristic of tubes made out of this material is the hig.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EL550 55 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C @Temperature 20.0 °C |
83.3 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EL550 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | z, above Tg; IPC TM-650 2.4.24 |
Arlon 84N Polyimide Laminate and Prepreg 84N is a high performance ceramic-filled polyimide prepreg based on Arlon's 85N pure polyimide system, designed for use in filling etched areas in polyimide multilayers that contain thick copper lay.. |
|||
CTE, linear, Transverse to Flow | 150 - 150 µm/m-°C @Temperature 60.0 - 138 °C |
83.3 - 83.3 µin/in-°F @Temperature 140 - 280 °F |
Average value: 150 µm/m-°C Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |