Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 136 µm/m-°C @Temperature 23.0 - 60.0 °C |
75.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp WFL32 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFL32 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 136 µm/m-°C @Temperature 23.0 - 60.0 °C |
75.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp RF00AES PA 66 (Europe-Africa-Middle East) LNP THERMOCOMP* RF00AES is a compound based on PA66 resin containing Glass Fiber, Mold Release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 136 µm/m-°C @Temperature 23.0 - 60.0 °C |
75.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RF00AES PA66/6, 50% Glass Filled, Injection Molded Staramide RF00AES is a 50% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 50V S3)Information provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 136 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
75.6 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359 |
Ascend Performance Materials Vydyne® 47 Nylon 66, DAM Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st.. |