Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 13.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
7.22 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP510A Glass Fabric Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-.. |
|||
CTE, linear, Transverse to Flow | 13.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
7.22 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP634 Laminate Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and.. |
|||
CTE, linear, Transverse to Flow | 13.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
7.22 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP660 Paper Base Laminate Description: Lower cost paper phenolic NEMA Grade XP. Uses natural kraft paper without pigmented cover sheet. Warm to hot punching. UL listed. Thickness Tested: 0.062", 0.125" & 0.500" |
|||
CTE, linear, Transverse to Flow | 13.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
7.22 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis |
Industrial Laminates/Norplex P95 Glass Fabric Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested.. |
|||
CTE, linear, Transverse to Flow | 13.0 µm/m-°C @Temperature 23.0 °C |
7.22 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-20A Samarium Cobalt Magnetic Material |
|||
CTE, linear, Transverse to Flow | 13.0 µm/m-°C @Temperature 23.0 °C |
7.22 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-20B Samarium Cobalt Magnetic Material |
|||
CTE, linear, Transverse to Flow | 13.0 µm/m-°C @Temperature 23.0 °C |
7.22 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-26A Samarium Cobalt Magnetic Material |
|||
CTE, linear, Transverse to Flow | 13.0 µm/m-°C @Temperature 23.0 °C |
7.22 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-22A Samarium Cobalt Magnetic Material |
|||
CTE, linear, Transverse to Flow | 13.0 µm/m-°C @Temperature 23.0 °C |
7.22 µin/in-°F @Temperature 73.4 °F |
|
Alliance S-22B Samarium Cobalt Magnetic Material |