Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® KU 1-7301 000000 PBT PBT, non-reinforced, injection molding, food contact |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® S 7926 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 60.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP (Europe-Africa-Middle East) LNP* Thermocomp* MB006S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 60.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP MB006SXP PP (Europe-Africa-Middle East) LNP* Thermocomp* MB006SXP is a compound based on Polypropylene resin containing Glass Bead. Added featurs include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 80.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East) VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Akulon® Fuel Lock FL-LP PA6 Low fuel permeation PA6 suitable for use in injection molding/welding of small engine fuel tanks, UV stabilized |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-E7300 PA410-I Tube Extrusion |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 X black PA612-I Product Description: Grilamid 2D 25 W 20 X black 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique proper.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® EB 50 H PA6 Product description: Grilon EB 50 H is a high viscosity, unreinforced, heat stabilized PA6 extrusion blow mounding grade. Grilon EB 50 H has the following important properties: High melt strengthImp.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® EBV-15H black 9697 PA6-GF15 Product description: Grilon EBV-15H black 9697 is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 15% glass fibers. Grilon EBV-15H black 9697 has the following important prop.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50 Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 3915 PA12-GF50 Product description: Grilamid XE 3915 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following produce profile:Good UV StabilityHigh impact strengthVe.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100TE NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100TE NC010 (formerly DE20580) is a high viscosity toughened acetal homopolymer with very low VOC emissions. Processing met.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 60.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 80G14AHS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS NC010 is a 14% glass fiber reinforced toughened high flow heat stabilized polyamide 66 resin. It offers outstanding perform.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® M25-44/M25S Acetal Co-polymer (POM), Standard, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |