Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 12.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.00 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON 9X06519 Cyclic Olefinic Copolymer LNP STAT-KON* 9X06519 is a compound based on Cyclic Olefinic Copolymer resin containing 30% Carbon Fiber. Added features of this material include: Clean Compounding System, Electrically Conductive... |
|||
CTE, linear, Transverse to Flow | 12.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.00 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON 9X06519 Cyclic Olefinic Copolymer (Asia Pacific) LNP STAT-KON* 9X06519 is a compound based on Cyclic Olefinic Copolymer resin containing Carbon Fiber. Added features of this material include: Clean Compounding System. |