Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 119 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR6300 AES+PC+SAN (Asia Pacific) Wear resistant PC+SAN, with proprietary lubricant, for business equipment applications. |
|||
CTE, linear, Transverse to Flow | 119 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY Lexan_WR6300 AES+PC+SAN LNP* Lubriloy* Lexan_WR6300 compound is a wear resistant PC+SAN, with proprietary lubricant, for business equipment applications. |
|||
CTE, linear, Transverse to Flow | 119 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON IS000XXL PA6.12 LNP* STAT-KON* IS000XXL is a compound based on Nylon 6/12 containing Stainless Steel Fibers. Added features of this material include: Food Contact Compliant Raw Materials, Metal Detectable, Electr.. |
|||
CTE, linear, Transverse to Flow | 119 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Stat-kon IS000LX PA6.12 LNP* Stat-Kon* IS000LX is a compound based on Nylon 6/12 containing Stainless Steel Fibers.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 119 µm/m-°C @Temperature 23.0 - 60.0 °C |
66.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON KEL22A Acetal Homopolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KEL22A is a compound based on Acetal Homopolymer resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 119 µm/m-°C | 66.1 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope.. |
|||
CTE, linear, Transverse to Flow | 119 µm/m-°C | 66.1 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |