Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 102 µm/m-°C @Temperature 23.0 - 60.0 °C |
56.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing milled Glass and PTFE. Added features include; Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 102 µm/m-°C @Temperature 23.0 - 60.0 °C |
56.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RX94033 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RX94033 is a compound based on PA 66 resin containing Aramide Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 102 µm/m-°C @Temperature -30.0 - 30.0 °C |
56.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP VC006 SUPER TOUGH NYLON LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon resin containing 30% Carbon Fiber. Added features of this material include: High Impact, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 102 µm/m-°C @Temperature -30.0 - 30.0 °C |
56.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT LNP* THERMOCOMP* WF004 is a compound based on PBT resin containing 20% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 102 µm/m-°C @Temperature -30.0 - 30.0 °C |
56.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6 LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon 6/6 resin containing Carbon Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Transverse to Flow | 102 µm/m-°C @Temperature -40.0 - 37.8 °C |
56.7 µin/in-°F @Temperature -40.0 - 100 °F |
ASTM E831 |
Diamond Polymers DIAMALOY GLY FXW749 Sheet Extrusion Grade, Sparkle/Pearlescence Diamaloy GLY FXW749SK resin is a low impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging and added visual effects (pearlescence). It has good melt strength for.. |
|||
CTE, linear, Transverse to Flow | 102 µm/m-°C @Temperature 23.0 - 60.0 °C |
56.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 102 µm/m-°C @Temperature 23.0 - 60.0 °C |
56.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG3ST43 PA6, 15% Glass Fiber Filled, Impact Modified, Injection Molded BG3ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |