Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow) |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Lanxess Pocan® BF 4232 HR 901510 PBT, 30% Glass Fiber PBT, 30% glass fiber, injection molding, flame retardant, hydrolysis stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36S PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duranex® 2000 Polybutylene Terephthalate (PBT), High flow DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duranex® 2002U Polybutylene Terephthalate (PBT), Weather resistance DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® F126-C Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Akulon® F-X9183 PA6 Low/Medium Viscosity |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BGZ-50/2 PA6-I-GF50 Information provided by EMS Grivory |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® EBGM-20 HX PA666-GF15 Product description: Grilon EBGM-20 HX black 9992 is a high viscosity, high heat stabilized PA66 + PA6 extrusion blow molding grade with 15% glass fibers. The special features of Grilon EBGM-20 HX b.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-2H black PA*-GF20 Product description: Grivory GV-2H is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide. Grivory.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSGZ-25/4 PA666-GF25 Information provided by EMS Grivory |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30 Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal (POM)
(Unverified Data**) Nucleated High Viscosity Acetal Homopolymer Developed for Extrusion Delrin 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability low die deposi.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100KM NC000 Acetal (POM)
(Unverified Data**) Kevlar® Modified High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100KM is a high viscosity acetal homopolymer resin modified with Kevlar aramid resin. It is designed for appl.. |