Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 489 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 254 °C

@Thickness 3.20 mm
489 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics EXTEM XH2315 TPI Resin
Extem XH2315 Resin
Deflection Temperature at 1.8 MPa (264 psi) 254 °C

@Thickness 3.20 mm
489 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Asia Pacific)
Extem XH2315 Resin
Deflection Temperature at 1.8 MPa (264 psi) 254 °C

@Thickness 3.20 mm
489 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Europe-Africa-Middle East)
Extem XH2315 Resin