Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 406 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 208 °C

@Thickness 6.40 mm
406 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics ULTEM 2210EPR PEI
20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
Deflection Temperature at 1.8 MPa (264 psi) 208 °C

@Thickness 6.40 mm
406 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
Deflection Temperature at 1.8 MPa (264 psi) 208 °C

@Thickness 3.20 mm
406 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics ULTEM UC1200 PEI (Asia Pacific)
12% carbon fiber reinforced Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 listing in recognized colors.
Deflection Temperature at 1.8 MPa (264 psi) 208 °C

@Thickness 3.20 mm
406 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI
LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications.
Deflection Temperature at 1.8 MPa (264 psi) 208 °C

@Thickness 3.20 mm
406 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI (Europe-Africa-Middle East)
LNP* Stat-kon* Ultem_UC1200 compound is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications.
Copyright © lookpolymers.com All Rights Reserved