Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 206 °C @Thickness 3.20 mm |
403 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM 2210EPR PEI 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 206 °C @Thickness 3.20 mm |
403 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |