Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 4.00 mm |
289 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1200-03 Polycarbonate Resin Description: LUPOY PC 1200-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 4.00 mm |
289 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1201-05 Polycarbonate Resin Description: LUPOY PC 1201-05 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 4.00 mm |
289 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1261-03 Polycarbonate Resin Description: LUPOY PC 1261-03 resin is designed for extrusion blow molding(EBM) and injection stretch blow molding (ISBM) products. It exhibits an excellent physical property balance of heat resista.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 4.00 mm |
289 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 4.00 mm |
289 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1600-03 Polycarbonate Resin Description: LUPOY PC 1600-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 4.00 mm |
289 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1603-03 Polycarbonate Resin Description: LUPOY PC 1603-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 4.00 mm |
289 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1300-03 Polycarbonate Resin Description: LUPOY PC 1300-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |