Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 104 °C @Thickness 6.35 mm |
219 °F @Thickness 0.250 in |
annealed, 120°C/hr; ASTM D648 |
Chi Mei Kibisan® PN137H SAN Resin, General Purpose Information provided by Calsak Corporation |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 104 °C @Thickness 3.18 mm |
219 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ CPVC LC500 Polyvinyl Chloride, Chlorinated (CPVC) Geon LC500 CPVC is an extrusion grade rigid compound. It is designed for applications where enhanced resistance at elevated temperatures is needed. LC500 demonstrates ease of processing with excelle.. |