Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 3.20 mm |
203 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycolac® X17 ABS Automotive: Very high heat resistance with high strength and modulus. UL94 HB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 6.40 mm |
203 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 6.40 mm |
203 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 3.20 mm |
203 °F @Thickness 0.126 in |
Annealed; ASTM-D648 |
Ineos ABS Lustran® 308 ABS, Medical Grade Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 6.35 mm |
203 °F @Thickness 0.250 in |
unannealed, 120°C/hr; ASTM D648 |
Chi Mei Kibisan® PN137H SAN Resin, General Purpose Information provided by Calsak Corporation |